Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.52 J/cm | 6.59 ft-lb/in | ASTM D256 |
Rotuba MSS Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 3.52 J/cm | 6.59 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 12% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Izod Impact, Notched | 3.52 J/cm | 6.59 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 12% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Izod Impact, Notched | 3.52 J/cm | 6.59 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Izod Impact, Notched | 3.52 J/cm | 6.59 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Izod Impact, Notched | 3.52 J/cm @Temperature 23.0 °C |
6.59 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp 2C003 LNP* Thermocomp* 2C003 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was su.. |
|||
Izod Impact, Notched | 3.52 J/cm | 6.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP 2C003 ETFE LNP* THERMOCOMP* 2C003 is a compound based on ETFE resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 3.52 J/cm | 6.59 ft-lb/in | Method B; Ductile Failure |
Elastomer Engineering Elastamide 100 Elastomer Modified RIM Nylon 6 30% crystallinity. Information supplied by Elastomer Engineering. |
|||
Izod Impact, Notched | 3.52 J/cm | 6.59 ft-lb/in | Approximation; ISO 180/1U |
Albis Plastics Tedur® L 9510-1 PPS, 40% Glass Fiber High Strength, High Rigidity Standard Grade. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Pump Impellers, Valve Housings and BushingsProcessing: Injection Molding (.. |
|||
Izod Impact, Notched | 3.52 J/cm | 6.59 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 12% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Izod Impact, Notched | 3.52 J/cm | 6.59 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |