Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.270 - 3.50 J/cm | 0.506 - 6.56 ft-lb/in | Average value: 0.801 J/cm Grade Count:26 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Izod Impact, Notched | 0.427 - 3.50 J/cm | 0.800 - 6.56 ft-lb/in | Average value: 0.972 J/cm Grade Count:56 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Notched | 0.267 - 3.50 J/cm | 0.500 - 6.56 ft-lb/in | Average value: 0.554 J/cm Grade Count:32 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Notched | 0.5339 - 3.50 J/cm @Temperature -40.0 - 0.000 °C |
1.000 - 6.56 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 1.23 J/cm Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||
Izod Impact, Notched | 0.534 - 3.50 J/cm | 1.00 - 6.56 ft-lb/in | Average value: 2.10 J/cm Grade Count:24 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |