Mechanical Properties Metric English Comments
Izod Impact, Notched 3.47 J/cm

@Temperature 23.0 °C
6.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products FT4700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
ASTM D-256
PlastiComp Complet® LGF50 - PA6 Nylon 6, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
ASTM D-256
PlastiComp Complet® LGF50-PPA Polyphthalamide, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyphthalamide with 50% long glass fiber reinforcementInformation provided by PlastiC..
Izod Impact, Notched 3.47 J/cm

@Temperature 23.0 °C
6.50 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycolac® MG37CR ABS
High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 3.47 J/cm

@Temperature 23.0 °C
6.50 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycolac® MG37CR ABS (Asia Pacific)
High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycolac® MGABS01 ABS
Injection molding ABS. High impact, high gloss, good flow.
Izod Impact, Notched 3.47 J/cm

@Temperature -30.0 °C
6.50 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer
PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
Method A; ASTM D256
Phillips 66 COPYLENE® CR020CL Polypropylene Impact Copolymer
COPYLENE® CR020CL is a random copolymer formulated with advanced clarifier technology and with antistat and is specially designed to excel in extrusion blowmolding processes. EBM bottles will have ..
Izod Impact, Notched 3.47 J/cm

@Temperature -30.0 °C
6.50 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Asia Pacific)
PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
ASTM D256
SABIC Innovative Plastics PREVEX W20 PPE+PS (Asia Pacific)
Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F.
Izod Impact, Notched 3.47 J/cm

@Thickness 3.17 mm
6.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® ASA 814 GY
Availability: North AmericaForms: PelletsFeatures: Good Weather ResistanceAppearance: GrayInformation provided by TP Composites, Inc.
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
Saint-Gobain Rulon® DC7035 Bearing/Seal PTFE
Offers electrical conductivity in a low wear, self lubricating bearing material. This material is ideal in applications where static dissipation is needed. DC7035 is often used as a static bleed mec..
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL PN235 PPE+PS
Plating grade, primarily automotive applications.
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL PN235 PPE+PS (Asia Pacific)
Plating grade, primarily automotive applications.
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL EM7100 PPE+PS
Automotive interiors. 200F DTUL. Excellent processability/economy. Good impact/mechanicals vs styrenics. Trim/instrument panel components.
Izod Impact, Notched 3.47 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
6.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
bar; ASTM D256
Diamond Polymers ABS 3001MC
Description: Plating GradeInformation provided by Diamond Polymers, Inc.
Izod Impact, Notched 3.47 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
6.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
bar; ASTM D256
Diamond Polymers ABS 3002MC
Description: Plating GradeInformation provided by Diamond Polymers, Inc.
Izod Impact, Notched 3.47 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
6.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Diamond Polymers ABS 3501 Black 1302 Injection Molding Grade
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 3.47 J/cm

@Temperature 22.8 °C
6.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Clariant Renol PCSP0005 Polycarbonate/ASA Alloy, Flame Retardant
Data provided by Clariant Masterbatches
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® P268WO PPO
An extrusion grade for general purpose application requiring flame retardancy and good impact resistance.Data provided by the manufacturer
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON MFD03 PP
LNP* STAT-KON* MFD03 is a compound based on Polypropylene resin containing 15% Glass Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON MFD03 PP (Asia Pacific)
LNP* Stat-kon* MFD03 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
ASTM D256
SABIC Innovative Plastics PREVEX W20 PPE+PS
Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F.
Izod Impact, Notched 3.47 J/cm

@Thickness 3.17 mm
6.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA12 1100 Tungsten Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Tungsten FillerInformation provided by TP Composites, Inc.