Polymer Property : Izod Impact, Notched = 6.35 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 6.35 J/cm
11.9 ft-lb/in
ASTM D256
DuPont™ Surlyn® 8920 Ionomer Resin, Sodium
Surlyn® 8920 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Izod Impact, Notched 6.35 J/cm
11.9 ft-lb/in
ASTM D256
DuPont™ Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium
Surlyn® PC100 luxury molding resin is a "select" grade of Surlyn® 8920, controlled to achieve the highest possible optical clarity in molded perfume jars and caps. It complies with the provisions ..
Izod Impact, Notched 6.35 J/cm
11.9 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Copolymer CP0437C10L Calcium Reinforced