Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256-93a |
Multibase Multi-Pro® 4810 C White 47.7% Filler Content Polypropylene Moisture content is 0.04%. Data provided by Multibase. |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256-56 |
Rotuba 856, Slow Burning Ethyl Cellulose Data provided by the manufacturer. |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | 0.25 in; ASTM D256 |
Ravago Manufacturing Americas Hylac® GP55 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL SE100X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/V1 rated. RTI Elec/Imp/Str 95/80/95. Good flow. Suitable for E/E market indoor/outdoor applications. |
|||
Izod Impact, Notched | 2.56 J/cm @Thickness 3.17 mm |
4.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® ABS FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantTPCI# 1039121Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.56 J/cm @Thickness 3.17 mm |
4.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF8 IM4 HS L 8% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 8% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Compo.. |
|||
Izod Impact, Notched | 2.56 J/cm @Temperature 23.0 °C |
4.80 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp HX05073 PA 11 LNP THERMOCOMP* HX05073 is a compound based on Nylon 11 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 2.56 J/cm @Thickness 3.17 mm |
4.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.56 J/cm @Thickness 3.17 mm |
4.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.56 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
4.80 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
Compression Molded; ASTM D256 |
Teknor Apex APEX® RS 9011A Polyvinyl Chloride, Rigid Forms: PelletsInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA High flow PPO+PA. Power distribution box applications. |
|||
Izod Impact, Notched | 2.56 J/cm @Thickness 3.17 mm |
4.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON RVL28 PA 66 LNP* VERTON* RVL28 is a compound based on Nylon 66 resin containing 40% Long Glass Fiber, 10% PTFE. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant, Structura.. |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
Aclo Accucomp ABS ABS801L Medium Impact Grade |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® P254WO PPO A general purpose V-0 rated resin with high impact strength.Data provided by the manufacturer |
|||
Izod Impact, Notched | 2.56 J/cm @Thickness 3.18 mm |
4.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® HF-1006 Polyamide 11, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9086 (FDA Odor Mask), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP SF008 PA 12 (Asia Pacific) LNP* Thermocomp* SF008 is a compound based on Nylon 12 resin containing Glass Fiber. |
|||
Izod Impact, Notched | 2.56 J/cm @Temperature 23.0 °C |
4.80 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Verton NV006E PC/ABS LNP* Verton* NV006E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas region.. |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON NV006E PC/ABS (Asia Pacific) LNP* Verton* NV006E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON NV006E PC+ABS LNP* Verton* NV006E is a compound based on PC+ABS blend resin containing 30% Long Glass Fiber. Added features of this material include: Easy Molding, Structural. |
|||
Izod Impact, Notched | 2.56 J/cm @Thickness 3.17 mm |
4.80 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® B3WG6 BK00564 BGVW 30% Glass Filled PA6 (Conditioned) Ultramid B3WG6 BK00564 BGVW is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |