Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.65 J/cm @Thickness 3.20 mm |
8.71 ft-lb/in @Thickness 0.126 in |
reverse notched; ASTM D 256 |
SABIC Innovative Plastics Ultem 2200N PEI 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 4.65 J/cm @Thickness 3.20 mm |
8.71 ft-lb/in @Thickness 0.126 in |
reverse notched; ASTM D 256 |
SABIC Innovative Plastics Ultem 2200N PEI (Asia Pacific) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 4.65 J/cm @Thickness 3.20 mm |
8.71 ft-lb/in @Thickness 0.126 in |
reverse notched; ASTM D 256 |
SABIC Innovative Plastics Ultem 2200N PEI (Europe-Africa-Middle East) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |