Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.16 J/cm | 7.79 ft-lb/in | ASTM D256 |
Eastman Tenite Propionate 375E4000012 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 4.16 J/cm | 7.79 ft-lb/in | ASTM D256 |
Eastman Tenite Propionate 376E4000012 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 4.16 J/cm | 7.79 ft-lb/in | ASTM D256 |
Eastman Tenite Propionate 377E4861312 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 4.16 J/cm | 7.79 ft-lb/in | ASTM D256 |
Eastman Tenite Propionate 383A2R30012 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 4.16 J/cm | 7.79 ft-lb/in | ASTM D256 |
Eastman Tenite Propionate 358A4000008 Clear, Trsp Cellulose Acetate Propionate Plasticizer 14%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 4.16 - 5.23 J/cm | 7.80 - 9.80 ft-lb/in | |
Bulk Molding Compounds BMC T15(GPS) General Purpose Molding Compound BMC T15(GPS) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPS) is well suited for injection, transfer or compression.. |