Polymer Property : Izod Impact, Notched = 37.0 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.14 - 37.0 J/cm
4.00 - 69.3 ft-lb/in
Average value: 10.9 J/cm Grade Count:23
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..