Polymer Property : Izod Impact, Notched = 3.95 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.11 J/cm

@Temperature -30.0 °C
3.95 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL PX6120 PPE+PS
Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications.
Izod Impact, Notched 2.11 J/cm

@Temperature -30.0 °C
3.95 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Asia Pacific)
Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications.
Izod Impact, Notched 2.11 J/cm

@Temperature -30.0 °C
3.95 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Europe-Africa-Middle East)
Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications.
Izod Impact, Notched 2.11 J/cm
3.95 ft-lb/in
ASTM D256
Unitika M2350 PA6, Conditioned
Nano composite nylonInformation provided by Unitika Ltd.