Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.03 J/cm @Temperature 23.0 °C |
3.80 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products GC30P200-00 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 2.03 J/cm @Temperature 23.0 °C |
3.80 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products GC30P200-01 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 2.03 J/cm @Temperature 23.0 °C |
3.80 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products GC30P200-01UV 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black Applications: Interior componentsStructural housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 2.03 J/cm @Temperature 23.0 °C |
3.80 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products GC30P200-523 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, (GM 167A) Ebony Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 2.03 J/cm | 3.80 ft-lb/in | ASTM D-256 |
PlastiComp Velocity® LCF50-PA6 High Flow Nylon 6, 50% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Izod Impact, Notched | 2.03 J/cm | 3.80 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 29% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Izod Impact, Notched | 2.03 J/cm | 3.80 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9025 , 8% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF25 IM HS L BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI.. |
|||
Izod Impact, Notched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF14 IM4 HS L BKN 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Izod Impact, Notched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® HDPE E GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF33 BK 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Izod Impact, Notched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PP LGF50 CC NAT 12mm 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass Fiber, 50% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PC GF10 TS15 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: LubricatedAppearance: BlackInformation provided by T.. |
|||
Izod Impact, Notched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® Endura Control Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.03 J/cm | 3.80 ft-lb/in | ASTM D 638 |
Styrolution PS 6220 HIPS Excellent toughnessHigh glossDesigned for deep draw thermoformingInformation provided by Styrolution |
|||
Izod Impact, Notched | 2.03 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.80 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
Compression Molded; ASTM D256 |
Teknor Apex APEX® SRP 2700A Polyvinyl Chloride, Rigid Forms: Pellets Additional Information: HDT, Annealed; 24 hours, 156°FInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | 2.03 J/cm | 3.80 ft-lb/in | ASTM D256 |
Styron EMERGEâ„¢ 5710 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5710 advanced resin is an ignition resistant ABS resin with an excellent balance of flow and impact strength. Applications: Monitor Enclosures Surge Protectors and UPS Enclosures .. |
|||
Izod Impact, Notched | 2.03 J/cm | 3.80 ft-lb/in | ASTM Data |
Styron Magnum™ 344CC ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Izod Impact, Notched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® PA6/6 03003 CF Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact.. |
|||
Izod Impact, Notched | 2.03 J/cm | 3.80 ft-lb/in | ASTM D256 |
Westlake Plastics Ardel® Polyarylate Stock shapes extruded from Ardel resin are specifically formulated to endure the damaging effects of UV light. When exposed to UV light, this unique material undergoes a molecular rearrangement res.. |
|||
Izod Impact, Notched | 2.03 J/cm | 3.80 ft-lb/in | ASTM D256 |
Eastman Tenite Acetate 105E1R26033 Clear, Trsp Cellulose Acetate Plasticizer 29%. Weight loss on heating = 2.6% per ASTM D 707. Soluble matter loss = 0.4% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 2.03 J/cm | 3.80 ft-lb/in | ASTM D256 |
Eastman Tenite Propionate 383A2R30007 Natural, Trsp Cellulose Acetate Propionate Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Izod Impact, Notched | 2.03 J/cm @Temperature 22.8 °C |
3.80 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PA133G33 Nylon 66, 33% Glass Fiber, Highly Impact Modified Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 2.03 J/cm | 3.80 ft-lb/in | ASTM D256 |
Eastman Tenite Propionate 360E0096907 Natural, Trsp Cellulose Acetate Propionate Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness, .. |
|||
Izod Impact, Notched | 2.03 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
3.80 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 7407 Rigid PVC, Extrusion Georgia Gulf 7407 is a rigid PVC compound designed for outdoor applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 2.03 J/cm | 3.80 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 8% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 2.03 J/cm @Thickness 3.17 mm |
3.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® SER23 ABS General purpose and flame retarded ABS with excellent moldability and no plate-out.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Informat.. |