Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® MG38N ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature 22.8 °C |
7.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature 22.8 °C |
7.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-HH Polycarbonate, High Heat Polycarbonate, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resource.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D256 |
Global ABS-704 General Purpose High Impact ABS Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | |
MTI ThermoStran® PA66-40G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm |
7.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF50 IM2 L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact Modified and LubricantFeatures: Impact Modified and LubricatedProcessin.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics ABS405 Extrusion Grade ABS Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm |
7.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PA6/6,6 IM 6040 BK MB Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | -22°F; ASTM D256 |
Styron EMERGEâ„¢ 4410-18 MFR Polycarbonate EMERGEâ„¢ PC 4410-18 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l.. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
7.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ASA S170 Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D628 |
ACC EP WQS EPI Engineered Polymers Water Base Quick Set Epoxy EP WQS Water Base Quick Set, “Powered by Reactamine® Technology”, is a two component 60% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D256 |
Applied Composites 8033 Polyester SMC Industry Application: RecreationProduct Application: Sports EquipmentDistinct Features: Pigmentable, Low Cost, Good Weatherability, High Molding EfficiencyInformation provided by Applied Composites .. |
|||
Izod Impact, Notched | 3.74 - 5.34 J/cm | 7.00 - 10.0 ft-lb/in | |
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a.. |
|||
Izod Impact, Notched | 3.74 - 4.81 J/cm | 7.00 - 9.00 ft-lb/in | |
Bulk Molding Compounds BMC 5209-12940 Mineral Filled, Glass Reinforced Polyester BMC 5209-12940 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced.. |
|||
Izod Impact, Notched | 3.74 - 5340 J/cm | 7.00 - 10000 ft-lb/in | Average value: 4.50 J/cm Grade Count:9 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm |
7.01 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PolyOne Elastamax XL-0257-2 TPU-Based Thermoplastic Elastomer
(discontinued **) This is a general purpose thermoplastic elastomer based on TPU for injection molding, and has a high specific gravity for applications requiring high weight. Physical Form: Pellets. Standard Color.. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature 23.0 °C |
7.01 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Kleerdex Kydex® 107 Acrylic/PVC Thermoplastic Sheet
(discontinued **) High performance sheet for NSFApplications: Ice makers, vending machines, beverage dispensers, and other equipment requiring NSF approval, as a replacement for stainless steel parts where cost, weig.. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature 22.8 °C |
7.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
LTL Color Compounds ColorFast® GPA300 ABS Super-tough ABS with our highest impact strength, injection moldingAll information provided by LTL Color Compounders, Inc. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 3.74 - 13.9 J/cm @Temperature -50.0 - -50.0 °C |
7.01 - 26.0 ft-lb/in @Temperature -58.0 - -58.0 °F |
Average value: 8.37 J/cm Grade Count:3 |
Overview of materials for ABS/Polyurethane Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr.. |