Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.98 J/cm @Thickness 3.17 mm |
3.71 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Trimid® N6-TG30L-BK 30% Glass Fiber, High Impact Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | Approximation; ISO 180/1U |
Albis Plastics Tedur® L V 9400-1 PPS, 15% Carbon Fiber
(discontinued **) High Electrical and Thermal Conductivity, Long-term Anti-static Properties. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Clutch Components, BushingsProcessing: Inje.. |
|||
Izod Impact, Notched | 1.98 J/cm @Diameter 3.17 mm |
3.71 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 5511 High Impact Polystyrene Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Industrial productsProperties were determined on injection molded specimens at 23°C.. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
Eastman Tenite Butyrate 285A2R30016 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 8%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 733LD Nylon 6 A modified injection molding grade nylon for applications requiring flexibility.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.71 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |