Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.67 J/cm | 6.88 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX6120 PPE+PS Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Izod Impact, Notched | 3.67 J/cm | 6.88 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Asia Pacific) Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Izod Impact, Notched | 3.67 J/cm | 6.88 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Europe-Africa-Middle East) Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |