Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 3.42 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 3.42 J/cm
6.41 ft-lb/in
ASTM D-256
PlastiComp Complet® LGF50 - PP Homopolymer Polypropylene, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% long glass fiber reinforcementInformation provided by PlastiCom..
Izod Impact, Notched 3.42 J/cm
6.41 ft-lb/in
ASTM D-256
PlastiComp Complet® LGF60 - PP Homopolymer Polypropylene, 60% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 60% long glass fiber reinforcementInformation provided by PlastiCom..
Izod Impact, Notched 3.42 J/cm

@Thickness 3.17 mm
6.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
PlastxWorld CEVIAN® E10 Inherently Static Dissipative ABS
Inherently Static Dissipative ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Izod Impact, Notched 3.42 J/cm

@Temperature 0.000 °C
6.40 ft-lb/in

@Temperature 32.0 °F
ASTM D256
Formosa Plastics Formolene® 6501A Blow Molding and Injection Molding Polypropylene
Impact CopolymerApplications: Blow molded bottles and containers, blown and cast film applications, and profile extrusions such as corrugated board.Formolene 6501A is a medium impact copolymer with ..
Izod Impact, Notched 3.42 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
6.41 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Diamond Polymers ABS 4012B Blow Molding Grade
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 3.42 J/cm
6.40 ft-lb/in
ASTM D256
Aclo Accucomp ABS ABS846HL High Flow Medium Impact Grade
Izod Impact, Notched 3.42 J/cm
6.40 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Copolymer CP0437C30L Calcium Reinforced
Izod Impact, Notched 3.42 J/cm

@Thickness 3.17 mm
6.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Calsak CS-72L General Purpose ABS Resin
Product Characteristics:High Impact, High GlossInjection molding grade
Izod Impact, Notched 3.42 J/cm
6.40 ft-lb/in
ASTM D256
Multibase Multi-Flam™ 0803 LDPE NH Polyethylene
Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionUses:TubingPipingInformation provided by Multibase