Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.69 J/cm | 3.17 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34 PC LNP LUBRICOMP* DFL34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.69 J/cm | 3.17 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34H PC LNP LUBRICOMP* DFL34H is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Healthcare. |
|||
Izod Impact, Notched | 1.69 J/cm | 3.17 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON E9007E PEI LNP* VERTON* E9007E is a compound based on Polyetherimide (PEI) containing 35% Long Carbon Fiber. Added features of this grade include: Structural, High Temperature |
|||
Izod Impact, Notched | 1.69 J/cm | 3.17 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL EXNL0357 PPE+PS |