Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.67 J/cm | 3.13 ft-lb/in | ASTM D256 |
Kolon SPESIN® KP213G30SB3 Glass Fiber Reinforced PBT Compound Resin G/F 30% reinforcedApplications: Ignition coil bobbinsInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 1.67 J/cm | 3.13 ft-lb/in | |
Kuraray SEPTON® CM1 Compatibilizer Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo.. |
|||
Izod Impact, Notched | 1.67 J/cm @Temperature -30.0 °C |
3.13 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Izod Impact, Notched | 1.67 J/cm @Temperature -30.0 °C |
3.13 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Izod Impact, Notched | 1.67 J/cm @Temperature -30.0 °C |
3.13 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Izod Impact, Notched | 1.67 J/cm @Temperature -30.0 °C |
3.13 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Izod Impact, Notched | 1.67 J/cm @Temperature -30.0 °C |
3.13 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Izod Impact, Notched | 1.67 J/cm @Temperature -30.0 °C |
3.13 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Izod Impact, Notched | 1.67 J/cm | 3.13 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF006HL PC LNP THERMOCOMP* DF006HL is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Low Extractible, Healthcare. |
|||
Izod Impact, Notched | 1.67 J/cm | 3.13 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX2734 PPE+HIPS (Asia Pacific) PPE/HIPS, unfilled, FR-V1 |