Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 12.8 J/cm | 24.0 ft-lb/in | ASTM D256 |
Quantum Composites QC-8560 60% Glass Fiber Vinyl Ester SMC QC-8560 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It maintains excellent mechanical properties at temper.. |
|||
Izod Impact, Notched | 12.8 J/cm | 24.0 ft-lb/in | edgewise; ASTM D256 |
Haysite 54500 Polyester SMC, 35% Glass Reinforced A high strength fiberglass reinforced thermoset polyester compound formulated for injection, compression, or transfer molding. This material exhibits excellent electrical and mechanical properties, .. |
|||
Izod Impact, Notched | 12.8 J/cm | 24.0 ft-lb/in | ASTM D256 |
Clariant Renol PCSP0019 Polycarbonate/Acrylic Alloy Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 12.8 J/cm | 24.0 ft-lb/in | ASTM D256 |
Quantum Composites QC-8151C 55% Glass Fiber Vinyl Ester Static-Dissipative SMC
(discontinued **) QC-8151C is a vinyl ester sheet molding compound (SMC) designed for compression molding components requiring dimensional stability, resistance to high temperatures plus sufficient electrical conduct.. |