Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 11.2 J/cm | 21.0 ft-lb/in | |
Premix Premi-Glas® 1200-50VE 1200-50 VE SMC
(discontinued **) Description: Premi-Glas® 1200-50 VE is a sheet molding compound.Market: StructuralInformation provided by Premix. |
|||
Izod Impact, Notched | 11.2 J/cm | 21.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Izod Impact, Notched | 11.2 J/cm | 21.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Asia Pacific) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Izod Impact, Notched | 11.2 J/cm | 21.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Izod Impact, Notched | 11.2 J/cm | 21.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER PC+Polyester, UV Stabilized, Transparent |
|||
Izod Impact, Notched | 11.2 J/cm | 21.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Asia Pacific) PC+Polyester, UV Stabilized, Transparent |
|||
Izod Impact, Notched | 11.2 J/cm @Temperature 23.0 °C |
21.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Asia Pacific) Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b.. |
|||
Izod Impact, Notched | 11.2 J/cm @Temperature 23.0 °C |
21.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Europe-Africa-Middle East) Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b.. |
|||
Izod Impact, Notched | 11.2 J/cm | 21.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester, UV Stabilized, Transparent |
|||
Izod Impact, Notched | 11.2 J/cm | 21.0 ft-lb/in | ASTM D256 |
Applied Composites 8052 Polyester SMC Industry Application: RecreationProduct Application: Marine ProductsDistinct Features: High Strength, ResilientInformation provided by Applied Composites Corporation. |
|||
Izod Impact, Notched | 11.2 - 13.9 J/cm | 21.0 - 26.0 ft-lb/in | |
Bulk Molding Compounds BMC 680 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 680 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression and stuffer injection molding It is characterized by good moldability, very high impa.. |
|||
Izod Impact, Notched | 11.2 J/cm | 21.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX X8300CL PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester, UV Stabilized, Transparent, OQ Quality |