Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 20.85 J/cm @Thickness 3.20 mm |
39.06 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM EXUM0169 PEI Blend Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
Izod Impact, Notched | 20.85 J/cm @Thickness 3.20 mm |
39.06 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM EXUM0169 PEI Blend (Asia Pacific) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |