Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 10.1 - 10.7 J/cm @Thickness <=3.00 mm |
19.0 - 20.0 ft-lb/in @Thickness <=0.118 in |
ASTM D256A |
Plaskolite Mustang PETG Sheet MUSTANG sheet signage material is continually processed using Eastman Tritan® copolyester, MUSTANG offers superior forming details, improved material distribution and shorter heating and cooling cy.. |
|||
Izod Impact, Notched | 0.267 - 10.7 J/cm | 0.500 - 20.0 ft-lb/in | Average value: 3.01 J/cm Grade Count:13 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Izod Impact, Notched | 6.41 - 10.7 J/cm | 12.0 - 20.0 ft-lb/in | ASTM D256 |
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Izod Impact, Notched | 5.34 - 10.7 J/cm | 10.0 - 20.0 ft-lb/in | ASTM D256 |
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Izod Impact, Notched | 5.34 - 10.7 J/cm | 10.0 - 20.0 ft-lb/in | ASTM D256 |
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s.. |
|||
Izod Impact, Notched | 5.34 - 10.7 J/cm | 10.0 - 20.0 ft-lb/in | ASTM D256 |
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Izod Impact, Notched | 0.450 - 10.7 J/cm | 0.843 - 20.0 ft-lb/in | Average value: 3.69 J/cm Grade Count:4 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Izod Impact, Notched | 0.587 - 10.7 J/cm | 1.10 - 20.0 ft-lb/in | Average value: 2.31 J/cm Grade Count:11 |
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched | 5.34 - 10.7 J/cm | 10.0 - 20.0 ft-lb/in | ASTM D256 |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |