Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | ASTM D256 |
PolyMirae Moplen EP340K Sheet and Thermoforming Grade Polypropylene Moplen RP340K is the polypropylene random copolymer polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP340K is a random copolymer particularly suitable for.. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPESIN® KP213G15HI Multi Reinforced PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | ASTM D256 |
PolyMirae Moplen EP401M Injection Molding Grade Polypropylene Moplen EP401M is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP401M is a block copolymer particularly suitable for injection.. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical KEYFLEX BT GN7155F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2500A(W) PA6+GF50%, General Purpose Feature: Injection Molding, PA6+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2500B(W) PA66+GF50%, General Purpose Feature: Injection Molding, PA66+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 2.76 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HI2202B PP+GF20%, High Impact Description: Injection Molding, PP+GF20%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 65997-17-3 and 9010-79-1Information provided by LG Chemica.. |
|||
Izod Impact, Notched | >= 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 2.76 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HI5302RB PP+MF25%, High Impact Description: Injection Molding, PP+MF25%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN135HB30HI Multi Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | >= 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 2.76 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HI5302S PP+MF15%, High Impact Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsInformation provided by LG Chemical |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | |
Shinil Chemical SHINSTAT ABS Electrostatic Control Polymer Injection Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® LS-3302A PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® TX-0510 TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm |
2.76 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0812 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9130 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® TX-0510 TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® TX-0520T TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm |
2.76 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0812 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9130 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Tramid® 210G45 Polyamide, Reinforced Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G45 is a reinforced grade.Applications:Automotive gear level housingConnectors.. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® C501G40 Nylon 6, 40% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® LS-3302A PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trimma® SD6320 PMMA, Translucent High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and high hardnessInformat.. |
|||
Izod Impact, Notched | 1.47 J/cm @Temperature 23.0 °C |
2.76 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H6670B High Density Polyethylene Film Key Characteristics:High flowExcellent processabilityHigh stiffnessOdorlessSafe for food contactGood printabilityRecommended Applications: Bottles for drinking water, fruit juice, soft drink, milkI.. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | |
Zylog Hipolyene® 8025 HC Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | |
Zylog Hipolyene® 8110 EX Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) ST6010 Nylon 66 Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm |
2.76 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VS-0826 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® C501G40 Nylon 6, 40% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPELLOY® KB133G30 PC + PBT Alloy Resin
(discontinued **) SPELLOY® is a new technology of thermoplastic Polymer alloys developed to provide unique combination of excellent mechanical properties.High impact resistance (at low temperature), good dimensional.. |