Izod Impact, Notched 2.60 J/cm
4.87 ft-lb/in
ASTM D256
Nylene® 401, Nylon 6, at 50% Relative Humidity
Injection molding grade. Nylene 401 is recommended for general purpose nylon molding applications in both thin and heavy sections. Nylene 401 has high flow characteristics at minimal processing temp..
Izod Impact, Notched 2.60 J/cm
4.87 ft-lb/in
ASTM D256
Nylene® 404 Nylon 6, 50% RH
Injection molding grade. Nylene 404 is a heat stabilized version of 401 which is recommended for general purpose nylon molding applications in both thin and heavy sections. In addition to protection..
Izod Impact, Notched 2.60 J/cm
4.87 ft-lb/in
ASTM D256
Nylene® Norpex® AX235 PPE (Polyphenylene Ether)
Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Izod Impact, Notched 2.60 J/cm

@Temperature 23.0 °C
4.87 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Geloy XTWE265 ASA
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 2.60 J/cm
4.87 ft-lb/in
ASTM D256
SABIC Innovative Plastics GELOY XTWE265 ASA (Asia Pacific)
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.
Izod Impact, Notched 2.60 J/cm

@Temperature 23.0 °C
4.87 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Geloy XTWE265 ASA (Europe-Africa-Middle East)
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 2.60 J/cm
4.87 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer
6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability.
Izod Impact, Notched 2.60 J/cm
4.87 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Asia Pacific)
6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability.
Izod Impact, Notched 2.60 J/cm
4.87 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Europe-Africa-Middle East)
6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability.
Izod Impact, Notched 2.60 J/cm
4.87 ft-lb/in
Reverse notched; ASTM D256
LG Chemical LUCEL EC-610B Electrically Conductive POM, 10% Carbon Black Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Izod Impact, Notched 2.60 J/cm
4.87 ft-lb/in
ASTM D256-03
Ipiranga Petrochem GM 7040 G HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Izod Impact, Notched 2.60 J/cm

@Temperature -40.0 °C
4.87 ft-lb/in

@Temperature -40.0 °F
Partial Break; ASTM D256
Sterigenics Raprex® R-200 Branched High Density Polyethylene
Applications: Injection Molding and ExtrusionRAPREX® R-200 is a high density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its ..
Izod Impact, Notched 2.60 J/cm

@Temperature -40.0 °C
4.87 ft-lb/in

@Temperature -40.0 °F
Partial Break; ASTM D256
Sterigenics Raprex® R200D Branched High Density Polyethylene
Applications: Injection Molding and ExtrusionRAPREX® R200D is a high density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its ..
Izod Impact, Notched 2.60 J/cm

@Thickness 3.17 mm
4.87 ft-lb/in

@Thickness 0.125 in
ASTM Test
Styrolution Luran® S 776 SE ASA
Luran S 776 SE is a general purpose extrusion ASA grade with good toughness and strength, used for sheet and profile extrusions.Information provided by STYROLUTION, which is a joint venture between ..
Izod Impact, Notched 2.60 J/cm

@Temperature -20.0 °C
4.87 ft-lb/in

@Temperature -4.00 °F
ASTM D256
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific)
Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized
Izod Impact, Notched 2.60 J/cm

@Temperature 23.0 °C
4.87 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram RamShine PV1003 ABS, General Purpose
General purpose ABS for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 2.60 J/cm
4.87 ft-lb/in
ASTM-D256
Braskem GM5010T2B HDPE High Density Extrusion Polyethylene
GM5010T2B is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for water distribution. It is produced with bimodal technology and has high molar mass. ..