Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.25 J/cm | 2.34 ft-lb/in | ASTM D256 |
NCMT NanoPAC™ N12 High Performance Polypropylene Nanocomposite Characteristics: Less shrinkage Solved distortion problem Good balance in impact and stiffness High gloss Reduce production cycleApplications: Household Industry Toys IndustryInformation provided by.. |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -30.0 °C |
2.34 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -30.0 °C |
2.34 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Asia Pacific) Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -30.0 °C |
2.34 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® AD143 PC LEXAN AD143 is a medium viscosity, injection molding grade exhibiting low dust attraction. It is designed for applications with high optical requirements in terms of clarity and light transmission .. |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -30.0 °C |
2.34 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® AD143 PC (Europe-Africa-Middle East) LEXAN AD143 is a medium viscosity, injection molding grade exhibiting low dust attraction. It is designed for applications with high optical requirements in terms of clarity and light transmission .. |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -30.0 °C |
2.34 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® AD4820 PC (Europe-Africa-Middle East) LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin. |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -30.0 °C |
2.34 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPF1 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -30.0 °C |
2.34 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® LUX2489D PC (Europe-Africa-Middle East) Lexan LUX2489D is a polycarbonate resin with high reflective properties, UV additive, medium viscosity, injection molding grade exhibiting low dust attraction. |
|||
Izod Impact, Notched | 1.25 J/cm | 2.34 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP FARADEX DS0036I PC (Europe-Africa-Middle East) LNP* Faradex* DS0036I is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel Fiber. Added features of this material include: High Impact, Flame Retardant, Non-Bromin.. |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -30.0 °C |
2.34 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -30.0 °C |
2.34 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® AD4820 PC (Asia Pacific) LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin. |
|||
Izod Impact, Notched | 1.25 J/cm | 2.34 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP IFP36 PA6.12 LNP* LUBRICOMP* IFP36 is a Nylon 6/12 base resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of t his grade include: Wear Resistant. |
|||
Izod Impact, Notched | 1.25 J/cm | 2.34 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON WEF42I PBT LNP* STAT-KON* WEF42I is a compound based on PBT resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this grade include: High Impact, Electrically Conductive. |
|||
Izod Impact, Notched | 1.25 J/cm | 2.34 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC LNP* Thermocomp* DF004RXP is a compound based on Polycarbonate resin containing 20% Glass Fiber. Some light color grades may have lower impact data than natural and black. Added features include: .. |
|||
Izod Impact, Notched | 1.25 J/cm | 2.34 ft-lb/in | Natural & Black Colors; ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC LNP* Thermocomp* DF004RXP is a compound based on Polycarbonate resin containing 20% Glass Fiber. Some light color grades may have lower impact data than natural and black. Added features include: .. |
|||
Izod Impact, Notched | 1.25 J/cm | 2.34 ft-lb/in | Natural & Black Colors; ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC (Asia Pacific) 20% Glass Fiber Reinforced Polycarbonate. Some light color grades may have lower impact data than nature and black grade. |
|||
Izod Impact, Notched | 1.25 J/cm | 2.34 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP AB002 ABS LNP* THERMOCOMP* AB002 is a compound based on ABS resin containing 10% Glass Bead. |
|||
Izod Impact, Notched | 1.25 J/cm @Thickness 3.20 mm |
2.34 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 6503 High Impact Polystyrene Characteristics High Impact Available in various colors Easy flow High stiffness Processing Injection moldingApplications Computer cabinet, printer body, business machine housing etc. Material St.. |
|||
Izod Impact, Notched | 1.25 J/cm | 2.34 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature 23.0 °C |
2.34 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamSter PF300J50 PBT, 50% Glass Fiber + Glass beads 50% Glass-fiber and glass beads reinforced PBT.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.25 J/cm | 2.34 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.25 J/cm | 2.34 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.25 J/cm | 2.34 ft-lb/in | ASTM D256 |
UBE UBESTA® 3030UFX1 Rigid Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature 23.0 °C |
2.34 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTal PM8515 Acetal, High impact High impact polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.25 J/cm | 2.34 ft-lb/in | ASTM D256 |
Chem Polymer Chemlon 240 G Nylon 6, 43% Glass Fiber Reinforced A 43% glass fiber reinforced nylon 6, offering high rigidity and tensile strength, especially at high service temperatures.Data provided by the manufacturer, Chem Polymer. |
|||
Izod Impact, Notched | 1.25 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
2.34 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
Notched V 10 mm; ASTM D256 |
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer
(discontinued **) Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD.. |
|||
Izod Impact, Notched | 1.25 J/cm | 2.34 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -30.0 °C |
2.34 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -30.0 °C |
2.34 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Europe-Africa-Middle East) 25 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -30.0 °C |
2.34 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Europe-Africa-Middle East) 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized |