Polymer Property : Izod Impact, Notched = 2.32 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.24 J/cm

@Temperature 23.0 °C
2.32 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp 4X08423
LNP* Thermocomp* 4X08423 is a compound based on Perfluoroalkoxy Polymer (PFA) containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 1.24 J/cm
2.32 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10
LNP* THERMOCOMP* QF007 is a compound based on Nylon 6/10 resin containing 35% Glass Fiber.
Izod Impact, Notched 1.24 J/cm

@Temperature -30.0 °C
2.32 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL GFN3 PPE+PS
PPE+PS blend. 30% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui..