Polymer Property : Izod Impact, Notched = 2.29 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® LGK3020 PC (Asia Pacific)
Glass reinforced. Flame retardant.
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® LGK5030 PC (Asia Pacific)
Glass reinforced. Flame retardant.
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP FARADEX DS0036I PC
LNP* FARADEX* DS0036I is a compound based on Polycarbonate resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, No..
Izod Impact, Notched 1.22 J/cm

@Temperature 23.0 °C
2.29 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Faradex DS0036IP PC
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
Izod Impact, Notched 1.22 J/cm

@Temperature 23.0 °C
2.29 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Faradex DS0036IP PC (Asia Pacific)
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
Izod Impact, Notched 1.22 J/cm

@Temperature 23.0 °C
2.29 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Faradex DS0036IP PC (Europe-Africa-Middle East)
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC
LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing 20% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC (Asia Pacific)
LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated.
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Asia Pacific)
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Europe-Africa-Middle East)
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP EFL36XXC PEI
LNP* Lubricomp* EFL36XXC is a compound based on Polyetherimide containing 30% Glass Fiber, 155 PTFE. Characteristics of this grade are: Internally Lubricated.
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP PFN16 PA 6
LNP* LUBRICOMP* PFN16 is a compound based on Nylon 6 resin containing 30% Glass Fiber, 2% MOS2. Added features of this material include: Wear Resistant.
Izod Impact, Notched 1.22 J/cm

@Temperature 23.0 °C
2.29 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Lubricomp ZFL36CCX PPE+PS
LNP LUBRICOMP* ZFL36CCX is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for..
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66 (Europe-Africa-Middle East)
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Izod Impact, Notched 1.22 J/cm

@Temperature 23.0 °C
2.29 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Lubriloy RF206H PA 66
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Lubricant, Lubricants. Added features of this material include: Internally Lubricated.This data was su..
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRILOY RF206XXH PA 66
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC
LNP* Thermocomp* Lexan_LGK3020 compound is a glass reinforced. Flame retardant.
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC
LNP* Thermocomp* Lexan_LGN5030 compound is a glass reinforced. Flame retardant.
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC (Asia Pacific)
Glass reinforced. Flame retardant.
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC (Europe-Africa-Middle East)
LNP* Thermocomp* Lexan_LGK5020 compound is a glass reinforced, flame retardant material.
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6 (Asia Pacific)
LNP* Thermocomp* PF006U is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: UV Stabilized.
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP QF006 PA 6/10
LNP THERMOCOMP* QF006 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber.
Izod Impact, Notched 1.22 J/cm

@Temperature -30.0 °C
2.29 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL PX1278 PPE+PS
Primarily EXTRUSION material. Automotive. Passes FMVSS 302. Heat resistance of 130 C (266 F).
Izod Impact, Notched 1.22 J/cm

@Temperature 23.0 °C
2.29 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp DF002L PC (Asia Pacific)
LNP* THERMOCOMP* DF002L is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Low Extractible.This data was supplied by SABIC-IP for the Asia P..
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP QC006 PA 6/10 (Asia Pacific)
LNP* THERMOCOMP* QC006 is a compound based on Nylon 6/10 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Notched 1.22 J/cm

@Temperature -30.0 °C
2.29 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX626 PPE+PS+PA
Blowmolding and extrusion. High heat and chemical resistant.
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
Toyobo VYLOPET® EMC545 Injection Molding Polyester Resin, Glass Reinforced
Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo.
Izod Impact, Notched 1.22 J/cm

@Temperature 23.0 °C
2.29 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Lubricomp DCL36 PC
LNP LUBRICOMP* DCL36 is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP fo..
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC (Asia Pacific)
Glass reinforced. Flame retardant.