Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.380 - 10.3 J/cm | 0.712 - 19.3 ft-lb/in | Average value: 3.26 J/cm Grade Count:77 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |