Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.77 J/cm @Thickness 3.17 mm |
18.3 ft-lb/in @Thickness 0.125 in |
|
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 9.77 J/cm @Thickness 3.17 mm |
18.3 ft-lb/in @Thickness 0.125 in |
|
Mitsubishi Iupilon® E2000UR 5 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 9.77 J/cm @Thickness 3.17 mm |
18.3 ft-lb/in @Thickness 0.125 in |
|
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |