Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.20 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 9945A PC Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr.. |
|||
Izod Impact, Notched | 8.20 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 9945A PC (Asia Pacific) Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr.. |
|||
Izod Impact, Notched | 8.20 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 9945A PC (Europe-Africa-Middle East) Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr.. |
|||
Izod Impact, Notched | 8.20 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Asia Pacific) Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Izod Impact, Notched | 8.24 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Izod Impact, Notched | 8.24 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer (Asia Pacific) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Izod Impact, Notched | 8.24 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Izod Impact, Notched | 8.24 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb.. |
|||
Izod Impact, Notched | 8.24 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Asia Pacific) Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb.. |
|||
Izod Impact, Notched | 8.24 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb.. |
|||
Izod Impact, Notched | 8.24 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in ""Energy"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color pac.. |
|||
Izod Impact, Notched | 8.24 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in ""Energy"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color pac.. |
|||
Izod Impact, Notched | 8.20 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Izod Impact, Notched | 8.20 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Izod Impact, Notched | 8.20 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Izod Impact, Notched | 8.20 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Izod Impact, Notched | 8.24 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Izod Impact, Notched | 8.24 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Asia Pacific) Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Izod Impact, Notched | 8.24 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Izod Impact, Notched | 8.24 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9414T PC Copolymer (Asia Pacific) Lexan* EXL9414T resin grade is a halogen-free flame retardant polycarbonate featuring transparency, -40 degree C ductility and UL-94 V0 rating for injection molding applications. Excellent impact co.. |
|||
Izod Impact, Notched | 8.20 J/cm | 15.4 ft-lb/in | ASTM D256 |
IDI Composites M-205 Thermoset Polyester, Sheet MECHANICAL - Versatile family of compounds designed to meet a variety of mechanical, electro-mechanical, and corrosion applications. Outstanding structural properties at lowest possible costs.Data p.. |
|||
Izod Impact, Notched | 8.24 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY NX13401 PC+ABS LNP* STAT-LOY* NX13401 is a compound based on PC+ABS blend. Added features of this material include: Antistat, Flame Retardant, Excellent Release. |
|||
Izod Impact, Notched | 8.22 J/cm | 15.4 ft-lb/in | ASTM D256 |
Aclo Accucomp Polycarbonate POL050L Low Viscosity |
|||
Izod Impact, Notched | 8.24 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9414T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL9414T resin grade is a halogen-free flame retardant polycarbonate featuring transparency, -40 degree C ductility and UL-94 V0 rating for injection molding applications. Excellent impact co.. |
|||
Izod Impact, Notched | 8.20 J/cm | 15.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2071T PC Copolymer (Europe-Africa-Middle East) High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |