Mechanical Properties Metric English Comments
Izod Impact, Notched 7.60 J/cm
14.2 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® LUX9610 PC (Asia Pacific)
Lexan LUX9610 is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS require..
Izod Impact, Notched 7.60 J/cm
14.2 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® LUX9610 PC (Europe-Africa-Middle East)
Lexan LUX9610 is a UV stabilized flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance providing good colorstab..
Izod Impact, Notched 7.60 J/cm
14.2 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® ML7682 PC Copolymer (Asia Pacific)
Lexan ML7682 resin is a flame retardant polycarbonate blend featuring high flow, good processability, good impact, good heat resistance, and UV stability. It is of non-chlorine and non-bromine flame..
Izod Impact, Notched 7.60 J/cm
14.2 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® EXRL2032 PC (Asia Pacific)
Lexan EXRL2032 is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS requir..
Izod Impact, Notched 7.60 J/cm
14.2 ft-lb/in
ASTM D256
IDI Composites C-204 Thermoset Polyester, Sheet
CORROSION - (Patent pending). Versatile family of compounds designed for pressurized and thermo-mechanically stressed applications. Excellent corrosion resistance and high strength.Data provided by ..
Izod Impact, Notched 7.60 J/cm
14.2 ft-lb/in
ASTM D256
IDI Composites E-204 Thermoset Polyester, Sheet
ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista..
Izod Impact, Notched 7.58 J/cm

@Temperature 23.0 °C
14.2 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Valox® 350U PBT (Asia Pacific)
Impact modified, UV stabilised, flame retardant polyester with an internal glowwire rating of 850C on 1.6mm flat plaques.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 7.56 J/cm

@Thickness 3.17 mm
14.2 ft-lb/in

@Thickness 0.125 in
ASTM D256
Diamond Polymers DIAMALOY 530 PC/PBT Alloy, UV Stabilized/Weatherable
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 7.56 J/cm

@Thickness 3.17 mm
14.2 ft-lb/in

@Thickness 0.125 in
ASTM D256
Diamond Polymers DIAMALOY PCPBT 530 PC/PBT Alloy, UV Stabilized/Weatherable
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 7.60 J/cm
14.2 ft-lb/in
ASTM-D256
Braskem GM7746C HDPE Blow Molding Polyethylene
GM7746C is a high-density polyethylene specially developed for the manufacturing of blow molding fuel tanks. It has high molar mass and excellent mechanical properties. It also shows excellent tenac..
Izod Impact, Notched 7.60 J/cm
14.2 ft-lb/in
ASTM-D256
Braskem GM7746CA HDPE Blow Molding Polyethylene
GM7746CA is a high-density polyethylene specially developed for the manufacturing of blow molding fuel tanks. It has high molar mass and excellent mechanical properties. It also shows excellent tena..
Izod Impact, Notched 7.60 J/cm
14.2 ft-lb/in
ASTM D256
Braskem Green PE SGM7746C Blow Molding and Monofilament High Density Polyethylene
Lower greenhouse gas emissions100% made from renewable raw materialsPerformance and Competitiveness: Green Polyethylene has the same characteristics as petrochemical polyethyleneApplications: Mono..
Copyright © lookpolymers.com All Rights Reserved