Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 14.14 J/cm | 26.49 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY XTPM405 ASA+PC High flow PC/ASA with improved impact at room and low temperatures. Improved release. Excellent weatherability for outdoor unpainted or clearcoated applications. Injection Moldable with large color .. |