Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.97 J/cm | 3.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36 PC LNP* LUBRICOMP* DFL36 is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.97 J/cm | 3.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36HL PC (Asia Pacific) LNP* LUBRICOMP* DFL36HL is a compound based on Polycarbonate resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.97 J/cm | 3.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36XXP PC LNP* Lubricomp* DFL36XXP is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.97 J/cm @Temperature 23.0 °C |
3.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermotuf PC006I PA 6 (Asia Pacific) LNP* Thermotuf* PC006I is a compound based on Nylon 6 resin containing Carbon Fiber, Impact Modifier. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the.. |
|||
Izod Impact, Notched | 1.97 J/cm @Temperature 23.0 °C |
3.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl N190A PPE+PS (Asia Pacific) Low heat, flame retardant PPO/HIPS alloy. Internal flammability results only.Not a UL recognised material.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 1.97 J/cm @Temperature 23.0 °C |
3.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermotuf PC006I PA 6 LNP* Thermotuf* PC006I is a compound based on Nylon 6 resin containing Carbon Fiber, Impact Modifier. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the.. |
|||
Izod Impact, Notched | 1.97 J/cm | 3.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF V1000SU PA LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized. |
|||
Izod Impact, Notched | 1.97 J/cm | 3.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL 844 PPE+PS (Asia Pacific) Medium heat PPO/HIPS alloy used in the automotive industry. |
|||
Izod Impact, Notched | 1.97 J/cm | 3.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX0888 PPE+PS Unfilled, non-FR. Higher heat resistance than N110 (BOZ) and px0844 (USA). For automotive interiors. 250F (121C) DTUL. |
|||
Izod Impact, Notched | 1.97 J/cm | 3.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX0888 PPE+PS (Asia Pacific) Unfilled, non-FR. Higher heat resistance than N110 (BOZ) and px0844 (USA). For automotive interiors. 250F (121C) DTUL. |
|||
Izod Impact, Notched | 1.97 J/cm @Temperature 23.0 °C |
3.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermotuf V1000SU PA LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.97 J/cm | 3.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF V1000SU PA (Asia Pacific) LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized. |