Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.794 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.49 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCEL HI525L POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.794 J/cm | 1.49 ft-lb/in | ASTM D256 |
Cheng Yu Plastic SW15 POM/PTFE |
|||
Izod Impact, Notched | 0.796 J/cm | 1.49 ft-lb/in | 73°F; ASTM D256 |
Entec Hylox® 9230BK PBT, 30% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |