Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.200 - 0.680 J/cm @Temperature -40.0 - -20.0 °C |
0.375 - 1.27 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.416 J/cm Grade Count:3 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |