Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.4905 J/cm | 0.9189 ft-lb/in | JIS-K-6740 |
Denka VINYKON M1600 PVC, M grade for hard injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Izod Impact, Notched | 0.4905 J/cm | 0.9189 ft-lb/in | JIS-K-6740 |
Denka VINYKON M1610 PVC, M grade for hard injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Izod Impact, Notched | 0.4905 J/cm | 0.9189 ft-lb/in | JIS-K-6740 |
Denka VINYKON M2024 PVC, M grade for hard injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |