Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.907 J/cm @Thickness 3.18 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® UF-1006 FR HS LEX BK8-115 Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat Stabilized, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many L.. |
|||
Izod Impact, Notched | 0.907 - 8.01 J/cm | 1.70 - 15.0 ft-lb/in | Average value: 2.90 J/cm Grade Count:10 |
Overview of materials for PVC, Sheet Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Sheet Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Izod Impact, Notched | 0.907 J/cm @Thickness 3.18 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® EF-1004 BK8-115 Polyetherimide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Izod Impact, Notched | 0.907 J/cm @Thickness 3.18 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® STN-F-1006 HS Polyamide 46, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |
|||
Izod Impact, Notched | 0.907 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200X is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.907 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1285H Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1285H is a 20% glass reinforced copolymer polypropylene compound. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.907 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200X is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.907 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1285H Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1285H is a 20% glass reinforced copolymer polypropylene compound. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.907 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200X is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.907 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200X is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.907 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1285H Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1285H is a 20% glass reinforced copolymer polypropylene compound. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.907 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200X is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.907 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1285H Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1285H is a 20% glass reinforced copolymer polypropylene compound. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.907 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1285H Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1285H is a 20% glass reinforced copolymer polypropylene compound. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.907 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1285H Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1285H is a 20% glass reinforced copolymer polypropylene compound. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.907 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.70 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers NPP 808 C5 TDS Polycarbonate Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.907 J/cm | 1.70 ft-lb/in | ASTM D256A |
Dow DS6D81 Polypropylene Random Copolymer Resin OverviewConsistent processabilityGood optical propertiesLow temperature heat sealComplies with U.S. FDA 21 CFR 177.1520 (c)3.1a, Canadian HPFB No ObjectionDOW DS6D81 Polypropylene Resin is intended .. |
|||
Izod Impact, Notched | 0.907 J/cm | 1.70 ft-lb/in | ASTM D256A |
Dow DS6D82 Polypropylene Random Copolymer Resin OverviewConsistent processabilityGood optical propertiesLow temperature heat sealComplies with U.S. FDA 21 CFR 177.1520 (c)3.1aDOW DS6D82 Polypropylene Resin is intended for use as a heat seal coati.. |
|||
Izod Impact, Notched | 0.907 J/cm @Temperature -40.0 °C |
1.70 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
BASF Ultraform N 2640 Z4 UNC Q600 POM Ultraform N2640 Z4 UNC Q600 is a high toughness, elastomer-modified injection molding POM grade. |
|||
Izod Impact, Notched | 0.907 J/cm @Thickness 3.18 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Lubricomp® QFL-4536 Polyamide 6/10 Copolymer, Glass Fiber Reinforced, PTFE + Silicone Lubricant
(disconti Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Izod Impact, Notched | 0.907 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200X is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.907 J/cm @Thickness 3.18 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® SPS-F-1006 HS Syndiotactic Polystyrene, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |