Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.147 - 0.481 J/cm | 0.276 - 0.900 ft-lb/in | Average value: 0.259 J/cm Grade Count:10 |
Overview of materials for Acrylic, High Flow, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app.. |
|||
Izod Impact, Notched | 0.155 - 0.481 J/cm | 0.290 - 0.900 ft-lb/in | Average value: 0.286 J/cm Grade Count:4 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Izod Impact, Notched | 0.374 - 0.481 J/cm | 0.700 - 0.900 ft-lb/in | Average value: 0.423 J/cm Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be.. |
|||
Izod Impact, Notched | 0.320 - 0.481 J/cm | 0.600 - 0.900 ft-lb/in | ASTM D256 |
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon Offering improved tensile, compressive and flexural properties over conventional unfilled cast nylon, NYCAST® GF (Glass Filled)-30% provides increased load bearing characteristics and is the choice.. |
|||
Izod Impact, Notched | 0.160 - 0.481 J/cm | 0.300 - 0.900 ft-lb/in | Average value: 0.274 J/cm Grade Count:12 |
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max.. |