Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.843 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.350 - 0.450 J/cm
0.656 - 0.843 ft-lb/in
ASTM D256-06
Proto3000 Objet Digital Materials™ DM_4310 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
Izod Impact, Notched 0.350 - 0.450 J/cm
0.656 - 0.843 ft-lb/in
ASTM D256-06
Proto3000 Objet Digital Materials™ DM_4410 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
Izod Impact, Notched 0.350 - 0.450 J/cm
0.656 - 0.843 ft-lb/in
ASTM D256-06
Proto3000 Objet Digital Materials™ DM_4510 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
Izod Impact, Notched 0.350 - 0.450 J/cm
0.656 - 0.843 ft-lb/in
ASTM D256-06
Proto3000 Objet Digital Materials™ DM_4710 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
Izod Impact, Notched 0.300 - 0.450 J/cm

@Temperature -40.0 - -20.0 °C
0.562 - 0.843 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 0.363 J/cm Grade Count:2
Overview of materials for Polystyrene, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr..
Izod Impact, Notched 0.163 - 0.450 J/cm
0.305 - 0.843 ft-lb/in
Average value: 0.363 J/cm Grade Count:12
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum ..
Izod Impact, Notched 0.300 - 0.450 J/cm

@Temperature -40.0 - -40.0 °C
0.562 - 0.843 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.375 J/cm Grade Count:1
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Izod Impact, Notched 0.400 - 0.450 J/cm
0.749 - 0.843 ft-lb/in
ASTM D256
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection mo..
Izod Impact, Notched 0.400 - 0.450 J/cm
0.749 - 0.843 ft-lb/in
ASTM D256
Loxim 810 02T HB Polypropylene Compound, 10% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Izod Impact, Notched 0.350 - 0.450 J/cm
0.656 - 0.843 ft-lb/in
ASTM D256
Loxim 820 02T V0 Polypropylene Compound, 20% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Izod Impact, Notched 0.350 - 0.450 J/cm

@Temperature -40.0 - -40.0 °C
0.656 - 0.843 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.400 J/cm Grade Count:1
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..
Izod Impact, Notched 0.400 - 0.450 J/cm

@Temperature -40.0 - -20.0 °C
0.749 - 0.843 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 0.425 J/cm Grade Count:1
Overview of materials for Polypropylene with Glass Fiber + Bead Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max..
Copyright © lookpolymers.com All Rights Reserved