Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.834 J/cm | 1.56 ft-lb/in | ASTM D256 |
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Izod Impact, Notched | 0.834 J/cm | 1.56 ft-lb/in | ASTM D256 |
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Izod Impact, Notched | 0.834 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.56 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GN-2251BF Flame Retardant PA Alloy Feature: Injection Molding, Flame Retardant PA AlloyApplication: E&E partsInformation provided by LG Chemical |
|||
Izod Impact, Notched | 0.834 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.56 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High Gloss, Anti-scratchApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 9011-14-7 and 181028-79-5Informatio.. |
|||
Izod Impact, Notched | 0.834 J/cm | 1.56 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN133G20 G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | >= 0.834 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 1.56 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL LW4405 PP+GF/MF40% Description: Injection Molding, PP+GF/MF40%, Low WarpageApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0, 65997-17-3 and 12001-26-2Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.834 J/cm @Thickness 6.35 mm |
>= 1.56 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax CCP ABS/PBT 7320H-104 20% Glass Fiber Filled Product Description: A 20% glass fiber reinforced injection molding grade. Characteristics:Low warp age and excellent dimensionally stable Excellent electrical property Excellent mechanic and chemi.. |
|||
Izod Impact, Notched | >= 0.834 J/cm @Thickness 6.35 mm |
>= 1.56 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 3030-104 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Izod Impact, Notched | 0.834 J/cm | 1.56 ft-lb/in | ASTM D256 |
Cheng Yu Plastic N6G10 Nylon 6, 10% Glass Filled |
|||
Izod Impact, Notched | 0.834 J/cm | 1.56 ft-lb/in | ASTM D256 |
Cheng Yu Plastic N6GV10 Flame Retardant Nylon 6, 10% Glass Filled |
|||
Izod Impact, Notched | 0.834 J/cm | 1.56 ft-lb/in | ASTM D256 |
Cheng Yu Plastic NG1250S Nylon 66, 25% Glass Fiber Reinforced |
|||
Izod Impact, Notched | 0.834 J/cm | 1.56 ft-lb/in | ASTM D256 |
Cheng Yu Plastic IPS600 Flame Retardant HIPS |
|||
Izod Impact, Notched | 0.834 J/cm | 1.56 ft-lb/in | ASTM D256 |
Cheng Yu Plastic IPS601 Flame Retardant HIPS |
|||
Izod Impact, Notched | 0.834 J/cm | 1.56 ft-lb/in | ASTM D256 |
Cheng Yu Plastic IPS666N Electric Resisting HIPS |