Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.363 J/cm | 0.680 ft-lb/in | |
Abatron AboCast 8-8/Abocure 8-8 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 1 lb. (2.2 kg): 135 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F)... |
|||
Izod Impact, Notched | 0.363 J/cm | 0.680 ft-lb/in | ASTM D256 |
Kolon DIAMAT® EM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Izod Impact, Notched | 0.363 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.680 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP1000A PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.363 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.680 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP1000D PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.363 J/cm | 0.680 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® V230B 30% Mineral Filled Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Izod Impact, Notched | 0.363 J/cm | 0.680 ft-lb/in | |
Abatron AboCast 50-16/AboCure 50-17 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/28 ratio. Pot life: 500 g, 29 min. at 70°C (160°F). Exothermic Peak 242°C (468°F). Cures in 1-2 hrs at .. |