Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.270 - 0.630 J/cm | 0.506 - 1.18 ft-lb/in | Average value: 0.447 J/cm Grade Count:9 |
Overview of materials for Phenolic, Novolac, Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Notched | 0.500 - 0.630 J/cm | 0.937 - 1.18 ft-lb/in | Average value: 0.553 J/cm Grade Count:3 |
Overview of materials for PEKK, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Izod Impact, Notched | 0.270 - 0.630 J/cm @Temperature -40.0 - -40.0 °C |
0.506 - 1.18 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.395 J/cm Grade Count:11 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |