Mechanical Properties Metric English Comments
Izod Impact, Notched 0.147 - 0.481 J/cm
0.276 - 0.900 ft-lb/in
Average value: 0.259 J/cm Grade Count:10
Overview of materials for Acrylic, High Flow, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app..
Izod Impact, Notched 0.155 - 0.481 J/cm
0.290 - 0.900 ft-lb/in
Average value: 0.286 J/cm Grade Count:4
Overview of materials for Epoxy, High Temperature
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val..
Izod Impact, Notched 0.374 - 0.481 J/cm
0.700 - 0.900 ft-lb/in
Average value: 0.423 J/cm Grade Count:6
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be..
Izod Impact, Notched 0.320 - 0.481 J/cm
0.600 - 0.900 ft-lb/in
ASTM D256
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon
Offering improved tensile, compressive and flexural properties over conventional unfilled cast nylon, NYCAST® GF (Glass Filled)-30% provides increased load bearing characteristics and is the choice..
Izod Impact, Notched 0.160 - 0.481 J/cm
0.300 - 0.900 ft-lb/in
Average value: 0.274 J/cm Grade Count:12
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA)
This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max..