Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | >= 0.448 J/cm | >= 0.840 ft-lb/in | Method A; ASTM D 256 |
Karina E-854-10/390-B-ERYB White PVC Compound Heavy metal free PVC compound recommended for extrusion of profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | >= 0.448 J/cm | >= 0.840 ft-lb/in | Method A; ASTM D 256 |
Karina E 836-10/185-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | >= 0.448 J/cm | >= 0.840 ft-lb/in | Method A; ASTM D 256 |
Karina E 854-10/150-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | >= 0.448 J/cm | >= 0.840 ft-lb/in | Method A; ASTM D 256 |
Karina E 854-10/185-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | >= 0.448 J/cm | >= 0.840 ft-lb/in | Method A; ASTM D 256 |
Karina E 855-10/150-ERYB-PO White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 0.448 J/cm @Temperature 22.8 °C |
0.840 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Sinpolene GPP1615/2 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 15% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |
|||
Izod Impact, Notched | 0.448 J/cm | 0.840 ft-lb/in | ASTM D256 |
PlastxWorld Veroplas PB2001F Nylon 66 flame retarded (UL94 V0), unfilled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 0.448 J/cm | 0.840 ft-lb/in | ASTM D256 |
PlastxWorld Veroplas PB5300 Nylon 66 general purpose, 30% mineral filled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 0.448 J/cm | 0.840 ft-lb/in | ASTM D256 |
Aclo Accuguard Polypropylene HP0369V2CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Izod Impact, Notched | 0.448 J/cm | 0.840 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0334M40CL Mica Reinforced Coupled |
|||
Izod Impact, Notched | 0.448 J/cm | 0.840 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336C10L Calcium Reinforced |
|||
Izod Impact, Notched | 0.448 J/cm | 0.840 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336C20L Calcium Reinforced |
|||
Izod Impact, Notched | 0.448 J/cm | 0.840 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336C30L Calcium Reinforced |
|||
Izod Impact, Notched | 0.448 J/cm | 0.840 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336M10L Mica Reinforced |
|||
Izod Impact, Notched | 0.448 J/cm | 0.840 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339G20CL Glass Reinforced Coupled |
|||
Izod Impact, Notched | >= 0.448 J/cm | >= 0.840 ft-lb/in | Method A; ASTM D 256 |
Karina E 841-08/184-A-ERYB Beige PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 0.448 J/cm | 0.840 ft-lb/in | ASTM D256 |
Aclo Accutech SAN SAN930G30L Glass Reinforced |
|||
Izod Impact, Notched | >= 0.448 J/cm | >= 0.840 ft-lb/in | Method A; ASTM D 256 |
Karina E 841-08/184-Y-ERYB Beige PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |