Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.196 J/cm | 0.368 ft-lb/in | 0.250 inches; ASTM D256 |
Diapolyacrylate Acrypet® MF-001 PMMA Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers. |