Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.360 J/cm | 0.674 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, at 50% RH
(dis AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
Izod Impact, Notched | 0.360 J/cm @Thickness 6.35 mm |
0.674 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Edgetek® ES-15GF/000 RED Polyethersulfone - 15% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.360 J/cm | 0.674 ft-lb/in | ASTM D256A |
LyondellBasell Pro-fax 6301 Polypropylene Homopolymer, Flake Resin Primary Processing Method: Masterbatch/ConcentratesKey Features: general purpose polypropylene homopolymer flake resin, minimal stabilization, FDA acceptableApplications: compounding, concentrates, .. |
|||
Izod Impact, Notched | 0.360 J/cm | 0.674 ft-lb/in | ASTM D256/A |
Iran Petrochemical (PCC) 60507 High Density Polyethylene 60507 is a HDPE injection molding grade which combines good flowability with balanced physical properties. This resin is well suited for general purpose applications requiring high stiffness. Applic.. |
|||
Izod Impact, Notched | 0.360 J/cm | 0.674 ft-lb/in | |
Haveg 61NA Furfuryl Alcohol-Formaldehyde Resin A proprietary thermoset plastic consisting of a furfuryl alcohol-formaldehyde resin and non-asbestos silicate fillers. |
|||
Izod Impact, Notched | 0.360 J/cm | 0.674 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KX06415 Acetal Copolymer LNP LUBRICOMP* KX06415 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Powder. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Notched | 0.360 J/cm @Temperature 23.0 °C |
0.674 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp RL001 PA 66 LNP Lubricomp* RL001 is a Nylon 6/6 base resin containing PTFE lubricant. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.360 J/cm @Temperature 0.000 °C |
0.674 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 325FC PBT (Europe-Africa-Middle East) Commercial, VALOX 325FC is compliant with food contact regulations. VALOX 325FC is a general purpose, unreinforced PBT injection moulding resin which contains internal mold release. This new 325FC g.. |
|||
Izod Impact, Notched | 0.360 J/cm @Temperature -30.0 °C |
0.674 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 325FC PBT (Europe-Africa-Middle East) Commercial, VALOX 325FC is compliant with food contact regulations. VALOX 325FC is a general purpose, unreinforced PBT injection moulding resin which contains internal mold release. This new 325FC g.. |
|||
Izod Impact, Notched | 0.360 J/cm | 0.674 ft-lb/in | ASTM D256 |
SPS Guang Zhou SAMATâ„¢ 5508(f1) Flame-retarded Polypropylene Characteristic: Good flame resistance, weather resistance, good chemical resistance, high flow propertiesApplications: X'mas decorative product, E/E applianceInformation Provided by SPS (Guang Zhou).. |
|||
Izod Impact, Notched | 0.360 J/cm | 0.674 ft-lb/in | ASTM D256 |
SPS Guang Zhou SAMATâ„¢ 666(f1) Flame-retarded Polypropylene Characteristic: Flame retardance, weather resistance, good mechanical propertiesApplications: X'mas decorative product, E/E applianceInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Izod Impact, Notched | 0.360 J/cm | 0.674 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON RFD04 PA 66 LNP STAT-KON* RFD04 is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.360 J/cm | 0.674 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP CF008 PS LNP* THERMOCOMP* CF008 is a compound based on Polystyrene resin containing 40% Glass Fiber. |
|||
Izod Impact, Notched | 0.360 J/cm | 0.674 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP CX05470 PS LNP* THERMOCOMP* CX05470 is a compound based on Polystyrene resin containing 20% Glass Fiber. |
|||
Izod Impact, Notched | 0.360 J/cm @Temperature 23.0 °C |
0.674 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp QF002 PA6.10 LNP* Thermocomp* QF002 is a compound based on Nylon 6/10 containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.360 J/cm @Temperature -30.0 °C |
0.674 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Izod Impact, Notched | 0.360 J/cm @Temperature -30.0 °C |
0.674 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Asia Pacific) Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Izod Impact, Notched | 0.360 J/cm @Temperature -30.0 °C |
0.674 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an.. |
|||
Izod Impact, Notched | 0.360 J/cm | 0.674 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KAL22M Acetal Copolymer LNP LUBRICOMP* KAL22M is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Notched | 0.360 J/cm | 0.674 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP WCL36 PBT LNP* LUBRICOMP* WCL36 is a compound based on PBT resin containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Notched | 0.360 J/cm @Temperature -30.0 °C |
0.674 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
Izod Impact, Notched | 0.360 J/cm | 0.674 ft-lb/in | ASTM D256 |
Braskem JV060U Injection Molding High Density Polyethylene Boxes for beverages bottles; Boxes in general; Technical parts.Information provided by Braskem. |