Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.184 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.345 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Therma-Tech™ NJC-7500 Nylon 12
(discontinued **) PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.184 J/cm | 0.345 ft-lb/in | ASTM D256 |
Plenco 2308 Phenolic, Granular, Transfer Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Izod Impact, Notched | 0.184 J/cm | 0.345 ft-lb/in | ASTM D256 |
Plenco 2482 Phenolic, Granular, Transfer Molded PLENCO 02482 is a general purpose, organic filled phenolic molding compound offering excellent mechanical strength while maintaining dielectric properties at elevated humidity levels. UL recognized .. |
|||
Izod Impact, Notched | 0.184 J/cm | 0.345 ft-lb/in | ASTM D256 |
Plenco 3356 Phenolic, Granular, Compression Molded PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i.. |