Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.170 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.318 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Therma-Tech™ SF-4500 TC Polyphenylene Sulfide (PPS) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.170 J/cm @Temperature 23.0 °C |
0.318 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Konduit MT00EL PP LNP* Konduit* MT00EL is a Polypropylene base resin with thermal fillers. Characteristics of this grade are Thermal Conductivity and it is Low Extraactible.This data was supplied by SABIC-IP for th.. |
|||
Izod Impact, Notched | 0.170 J/cm | 0.318 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 LNP* Konduit* PX08322 is a compound based on PA6 resin containing mineral. Added features include: Thermally Conductive, Flame Retardant |
|||
Izod Impact, Notched | 0.170 J/cm | 0.318 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Izod Impact, Notched | 0.170 J/cm | 0.318 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN LNP* LUBRICOMP* BX03658N is a compound based on SAN resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerances, good for Water Meter A.. |
|||
Izod Impact, Notched | 0.170 J/cm | 0.318 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.170 J/cm | 0.318 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.170 J/cm | 0.318 ft-lb/in | ASTM D256 |
Plenco 3509 Phenolic, Granular, Injection Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |
|||
Izod Impact, Notched | 0.170 J/cm | 0.318 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.170 J/cm | 0.318 ft-lb/in | ASTM D256 |
Total PPH 3862 Homopolymer Polypropylene, Fiber Grade Total Petrochemicals Polypropylene 3862 is recommended for high speed melt spinning processes and multifilament yarns like bulk continuous filament (BCF) and continuous filament (CF) fibers. 3862 i.. |
|||
Izod Impact, Notched | 0.170 J/cm | 0.318 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.170 J/cm | 0.318 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.170 J/cm | 0.318 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.170 J/cm | 0.318 ft-lb/in | ASTM D256-10 |
DSM Somos® PerFORM Stereolithography Polymer, UV Postcure PerFORM produces strong, stiff, high-temperature resistant composite parts on standard 355 nm stereolithography machines. This material’s lower viscosity makes processing parts faster. It exhibits .. |
|||
Izod Impact, Notched | 0.170 J/cm @Temperature >=23.0 °C |
0.318 ft-lb/in @Temperature >=73.4 °F |
ASTM D256 |
Carmel Olefins CAPILENE® Y 50 V Polypropylene Homopolymer CAPILENE® Y 50 V is an ultra high melt flow rate polypropylene homopolymer suitable for thin walled injection molding and as a base resin for compounds applications. The product combines high stiff.. |
|||
Izod Impact, Notched | 0.170 - 0.270 J/cm | 0.318 - 0.506 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 132 Phenolic Molding Organic, inorganic, and graphite Filler, Compression Molded Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti.. |
|||
Izod Impact, Notched | 0.170 - 0.290 J/cm | 0.318 - 0.543 ft-lb/in | ASTM D256A |
DSM Somos® ProtoCast™ AF 19122 Antimony-free Liquid Photopolymer Product DescriptionDSM Somos® ProtoCast™ AF 19122 is an antimony-free liquid photopolymer specifically formulated for producing investment casting patterns.ApplicationsIdeal for use in foundry app.. |
|||
Izod Impact, Notched | 0.170 - 3.41696 J/cm @Temperature -20.0 - 4.00 °C |
0.318 - 6.40137 ft-lb/in @Temperature -4.00 - 39.2 °F |
Average value: 1.07 J/cm Grade Count:8 |
Overview of materials for Polypropylene, Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values.. |