Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.304 - 0.900 J/cm
0.570 - 1.69 ft-lb/in
Average value: 0.583 J/cm Grade Count:7
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched 0.304 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
0.569 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical Lupox® SG3180S PBT+PET+MF18%
Description: Injection Molding, PBT+PET+MF18%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical
Izod Impact, Notched 0.304 J/cm

@Temperature 23.0 °C
0.569 ft-lb/in

@Temperature 73.4 °F
ASTM D256
IRPC Polimaxx Polene 1111NX BA4 Polypropylene Compound
CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 20% BARIUM SULPHATE REINFORCED HIGH GLOSS APPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES
Izod Impact, Notched 0.304 J/cm
0.569 ft-lb/in
ASTM D256
E-Polymers SEPAZ® N2020L Nanoclay 2% High flow Nano Composite Resin
Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi..
Izod Impact, Notched >= 0.304 J/cm
>= 0.569 ft-lb/in
ASTM D256
Gromax Evasin EV-3201V Ethylene-Vinyl Alcohol Copolymer
Unmodified random Co-Polymer of [Ethylene-Vinyl alcohol], designed for therm-plastic processing into Sheets and Foils with high Oxygen and Aroma Barrier EffectInformation provided by Gromax Enterpri..