Polymer Property : Izod Impact, Notched = 0.294 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.157 - 0.534 J/cm
0.294 - 1.00 ft-lb/in
Average value: 0.280 J/cm Grade Count:13
Overview of materials for Acrylic, Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o..
Izod Impact, Notched 0.157 J/cm
0.294 ft-lb/in
ASTM D256
Lendell Parapet EH-1000 PMMA, Extrusion
Izod Impact, Notched 0.157 J/cm
0.294 ft-lb/in
ASTM D256
Lendell Parapet HH-1000L PMMA, Heat Resistant
Izod Impact, Notched 0.157 J/cm
0.294 ft-lb/in
ASTM D256
Plenco 5350 Phenolic, Granular, Compression Molded
PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties...