Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.147 - 11.0 J/cm | 0.276 - 20.6 ft-lb/in | Average value: 1.12 J/cm Grade Count:380 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Izod Impact, Notched | 0.147 - 0.481 J/cm | 0.276 - 0.900 ft-lb/in | Average value: 0.259 J/cm Grade Count:10 |
Overview of materials for Acrylic, High Flow, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app.. |
|||
Izod Impact, Notched | 0.147 J/cm | 0.276 ft-lb/in | ASTM D256 |
Lendell Parapet PMMA, High Flow |
|||
Izod Impact, Notched | 0.147 J/cm | 0.276 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® V200L Unfilled PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |