Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.147 J/cm | 0.275 ft-lb/in | 73°F; ISO 180 |
Multibase Multi-Pro® 2502 CU Black Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Izod Impact, Notched | 0.147 J/cm | 0.275 ft-lb/in | ASTM D256 |
LG Chemical EG920 PMMA, General Purpose Grade for Extrusion General purpose grade with excellent stress cracking resistanceIntended mainly for exterior applicationsRecommended mainly for sheets, pipes, and profilesFeatures: Excellent transparency and eleganc.. |
|||
Izod Impact, Notched | 0.147 J/cm | 0.275 ft-lb/in | ASTM D256 |
LG Chemical EH910 PMMA, General Purpose Grade for Extrusion Excellent solvent resistanceHighest of all grades in heat resistance, mechanical strength, surface hardness and stress cracking resistanceFeatures: Excellent transparency and eleganceWeather resista.. |
|||
Izod Impact, Notched | 0.147 J/cm | 0.275 ft-lb/in | ASTM D256 |
LG Chemical IF850 PMMA, General Purpose Grade for Injection Molding High flowability gradeParticularly recommended for complicated profiles or large and thin wall partsFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface har.. |
|||
Izod Impact, Notched | 0.147 J/cm | 0.275 ft-lb/in | ASTM D256 |
LG Chemical IF870S PMMA, General Purpose Grade for Injection Molding Highest flowability of all gradesFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface hardness and coloring propertySuperior electrical resistance and mecha.. |
|||
Izod Impact, Notched | 0.147 J/cm | 0.275 ft-lb/in | ASTM D256 |
LG Chemical IG840 PMMA, General Purpose Grade for Injection Molding General purpose grade with better flowability than IH 830 but slightly below in heat resistanceMechanical strength and surface hardnessFeatures: Excellent transparency and eleganceWeather resistance.. |
|||
Izod Impact, Notched | 0.147 J/cm | 0.275 ft-lb/in | ASTM D256 |
LG Chemical IH830A PMMA, General Purpose Grade for Injection Molding Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and .. |
|||
Izod Impact, Notched | 0.147 J/cm | 0.275 ft-lb/in | ASTM D256 |
LG Chemical IH830C PMMA, General Purpose Grade for Injection Molding Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and .. |
|||
Izod Impact, Notched | 0.147 J/cm | 0.275 ft-lb/in | ASTM D256 |
LG Chemical IH830H PMMA, General Purpose Grade for Injection Molding Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and .. |
|||
Izod Impact, Notched | 0.147 - 0.588 J/cm | 0.275 - 1.10 ft-lb/in | Average value: 0.309 J/cm Grade Count:10 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Izod Impact, Notched | 0.147 J/cm | 0.275 ft-lb/in | ASTM D256 |
LG Chemical IH830 PMMA, General Purpose Grade for Injection Molding Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and .. |